While used for applications similar to RNY309, its corrosion-resistance at normal temperature is equivalent to RYN316, and its crack-resistance is even better with the addition of Mo. Preferentially used for welding stainless clad steel and curing alloy steel for usage under normal temperature. The lime titania coating allows for welding in all positions.
Part Number |
---|
RNY309MO-3.2-5 |
RNY309MO-4.0-5 |
RNY309MO-5.0-5 |
Part Number | Price | Minimum Order Qty. | Volume Discount | Days to Ship | Rod Diameter (mm) | Current Range Downward (A) | Current Range Vertical Upward & Upward |
---|---|---|---|---|---|---|---|
₹ 19,908.75 | 1 Piece(s) | 8 Day(s) or more | 3.2 | 80–120 | 65~110 | ||
₹ 19,081.00 | 1 Piece(s) | 8 Day(s) or more | 4 | 110~150 | 85~135 | ||
₹ 19,052.87 | 1 Piece(s) | 8 Day(s) or more | 5 | 150~200 | - |
Part Number |
---|
Loading...
Product Model | Welding Rod | Rod Length(mm) | 350 | JIS standards | ES309Mo-16 Equivalent |
---|---|---|---|---|---|
AWS Standards | E309Mo-16 Equivalent | Mechanical Property : Tensile Strength(Mpa) | 650 (example, JIS standard: 550:≤) | Mechanical Property : 5D Extension(%) | 37.4 (example, JIS standard: 25:≤) |
Mechanical Property : Absorbed energy(J) | 82(20℃) | Identification Color | End Surface: Silver, Side Surface: - | Internal capacity | 1 Box (5 kg) |
Applications and Features | While used for application similar to RNY309, its corrosion-resistance under normal temperature is equivalent to RYN316, and crack-resistance is further superior by adding Mo. Preferred to be used for welding stainless clad steel and curing alloy steel for usage under normal temperature. Coating of lime titania type allows welding in any posture. | Ferrite Content: (Method) Schaeffler Organization Chart(%) | 15.0 | Cautionary Notes | Please dry at 150–200°C for approximately 1 hour prior to use. When welding, remove all oil, dust and other foreign material from the welding surface. |
How can we improve?
How can we improve?
Thank you for your time.
Your feedback is essential for our continuous improvement
Privacy Policy
Thank you for your cooperation.
Thank you for your time.
Your feedback is essential for our continuous improvement
Please use the inquiry form.
Privacy Policy